Nikasil block
Moderator: Team
Nikasil block
Hi, I recently saw a Nikasil plated steel alloy block that had the cylinder deck awfully looking.
I was told the deck it was ok and it just got that looking for the plating
Is that normal?
I was told the deck it was ok and it just got that looking for the plating
Is that normal?
-
- Expert
- Posts: 537
- Joined: Mon Dec 12, 2016 3:37 pm
- Location:
Re: Nikasil block
those marks are from a rotary abrasive tool of some sort, used to "prep" the deck for HG replacement.
they prepped it alright... for a trip to the resurfacing machine!
edit: looking closely I am seeing no circular marks as would be left from a rotary tool, but it looks very similar in nature. almost looks like a belt sander was used on it to be honest.
they prepped it alright... for a trip to the resurfacing machine!
edit: looking closely I am seeing no circular marks as would be left from a rotary tool, but it looks very similar in nature. almost looks like a belt sander was used on it to be honest.
-
- Pro
- Posts: 397
- Joined: Tue Dec 29, 2015 8:09 pm
- Location: TN
Re: Nikasil block
In those pictures the cylinders have been Nikasil plated and the deck looks like that after Nikasil treatment but before any cutting of the deck, correct? If that’s the finished product (decking included) that’s just plain wrong. A MLS gasket is not going to like that finish. If it’s ready for decking I’d be suspect on what procedures they used to clean the deck. That looks like someone with a chisel worked on that. I work on a lot of Nikasil coated Kohler tractor engines and the only think touched is the bores. I’ve never seen anything like that after treatment.
Re: Nikasil block
Looks like when someone hits a deck with sandpaper or a "cookie" because they don't like the look of the stains in the metal from where the old gasket was or wasn't.
It can be ugly as long as it is smooth and flat... and that deck is now neither!
It can be ugly as long as it is smooth and flat... and that deck is now neither!
-
- Guru
- Posts: 1564
- Joined: Thu Sep 16, 2010 10:01 am
- Location: Virginia
- Contact:
Re: Nikasil block
If the nikasil goes all the up to the deck, it probably should not be surfaced or the nickel will chip off. Maybe that's why it got cookie dusted.
"do it right or do it right away"
http://www.motionmachineinc.com/
https://www.youtube.com/watch?v=ZgIZbveknDs
http://www.motionmachineinc.com/
https://www.youtube.com/watch?v=ZgIZbveknDs
Re: Nikasil block
He just told me that the block deck is perfectly flat, but he isn't able to understand if it needs any machining on it.
If yes, is the Nikasil really going to chip off??
If yes, is the Nikasil really going to chip off??
-
- Guru
- Posts: 1564
- Joined: Thu Sep 16, 2010 10:01 am
- Location: Virginia
- Contact:
Re: Nikasil block
I do some blocks using iron Mahle nikasil sleeves. They warn to do no machining after installation for this reason.
"do it right or do it right away"
http://www.motionmachineinc.com/
https://www.youtube.com/watch?v=ZgIZbveknDs
http://www.motionmachineinc.com/
https://www.youtube.com/watch?v=ZgIZbveknDs
Re: Nikasil block
Sorry, are you referring to machining the block deck? Have you any email address to directly contact them about this? ThanksMotionMachine wrote: ↑Mon Nov 25, 2019 7:39 pm I do some blocks using iron Mahle nikasil sleeves. They warn to do no machining after installation for this reason.
-
- Guru
- Posts: 1564
- Joined: Thu Sep 16, 2010 10:01 am
- Location: Virginia
- Contact:
Re: Nikasil block
Yes, they say to not deck the top of the sleeve because the nickel goes all the way up and it might fracture if machined. I hone them of course but no decking. This was through engineers I do work for and their contact at Mahle Germany so I do not have any direct contact info for them.
"do it right or do it right away"
http://www.motionmachineinc.com/
https://www.youtube.com/watch?v=ZgIZbveknDs
http://www.motionmachineinc.com/
https://www.youtube.com/watch?v=ZgIZbveknDs
- midnightbluS10
- Expert
- Posts: 933
- Joined: Sun Oct 20, 2013 8:41 am
- Location: Shreveport, LA
Re: Nikasil block
What are cookies? Those little Scotch Brite Roloc pads that go on angle grinders?
JC -
bigjoe1 wrote:By the way, I had a long talk with Harold(Brookshire) last year at the PRI show. We met at the airport and he told me everything he knew about everything.It was a nice visit. JOE SHERMAN RACING
Re: Nikasil block
When the whole block goes to Nikasil/nicom plating, I think they mask the deck and it’s not plated. I think there’s a small chamfer still the top of the cylinder bore, and the plating ends somewhere there. At least for our blocks.
Paradigms often shift without the clutch -- https://www.youtube.com/watch?v=cxn-LxwsrnU
https://www.instagram.com/ptuomov/
Put Search Keywords Here
https://www.instagram.com/ptuomov/
Put Search Keywords Here
-
- Guru
- Posts: 1547
- Joined: Thu Sep 29, 2011 8:55 am
- Location:
Re: Nikasil block
Ive personally chipped a nikasil coated cylinder for a honda 450 single with a 3/4" carbide end mill taking 0.005" off the deck to tighten up the quench. Knocked a 0.020" x 0.020" or maybe less off. Was well short of the top ring. I ran it anyway with no issue.
-
- Guru
- Posts: 1762
- Joined: Wed Aug 26, 2009 8:30 pm
- Location: Beautiful Southern Maryland
- Contact:
Re: Nikasil block
https://www.enginerepairshop.com/abrasive-disc.htmlmidnightbluS10 wrote: ↑Sun Dec 01, 2019 1:02 pm What are cookies? Those little Scotch Brite Roloc pads that go on angle grinders?
Bill Koustenis
Advanced Automotive Machine
Waldorf Md
www.enginerepairshop.com
Advanced Automotive Machine
Waldorf Md
www.enginerepairshop.com